Chemical Suits - Kappler Zytron 500 - CE Certified Type 3 - Hood - Elastic Wrist/Ankle/Face
Zytron 500 is top of the class– and the classic responder choice. It’s tough, built for mobility, and based on patented technology that created the first material to survive eight full hours against the ASTM F1001 Test Battery with no breakthrough. With that kind of Kappler heritage built into the fabric, it’s no wonder that responders around the world trust Z500 garments for ultra-demanding Level A and Level B applications. Available in coveralls and a range of total encapsulating suits. Colors are Orange and Charcoal Gray.
Kappler Zytron 500 CE Certified Type 3 Coverall, Zipper Front, Attached Hood, Elastic Wrist, Ankles & Face Opening Color: Orange or Charcoal 3/case KA-Z5H428-OR-XS Orange Extra Small Heat Sealed/Taped Seams KA-Z5H428-OR-SM/MD Small/Medium KA-Z5H428-OR-LG/XL Large/XL KA-Z5H428-OR-2X/3X 2X/3X KA-Z5H428-OR-4X 4X
KA-Z5H428-CH-XS Charcoal Extra Small Heat Sealed/Taped Seams KA-Z5H428-CH-SM/MD Small/Medium KA-Z5H428-CH-LG/XL Large/XL KA-Z5H428-CH-2X/3X 2X/3X KA-Z5H428-CH-4X 4X
KAPPLER TECHNICAL DATA ASTM F1001 Chemical Test Battery
CHEMICAL
Zytron® 500
Acetone
>480
Acetonitrile
>480
Carbon Disulfide
>480
Dichloromethane
>480
Diethylamine
>480
Dimethylformamide
>480
Ethyl Acetate
>480
n-Hexane
>480
Methyl Alcohol
>480
Nitrobenzene
>480
Sodium Hydroxide
>480
Sulfuric Acid
>480
Tetrachloroethylene
>480
Tetrahydrofuran
>480
Toluene
>480
GASES
Ammonia Gas
>480
1,3 Butadiene
>480
Chlorine Gas
>480
Ethylene Oxide Gas
>480
Hydrogen Chloride Gas
>480
Methyl Chloride Gas
>480
NOTE: These tests were performed in accordance with ASTM standards by independent laboratories. This data is derived from tests performed on material samples only, not finished garments.
WARNING: There are uses, environments and chemicals for which these garments and/or fabrics are unsuitable. It is the responsibility of the user to review available data and verify that the garment and/or fabric is appropriate for the intended use and meets all specified government industry standards.
CAUTION: Do not use for fire protection. Avoid open flame or intense heat.
Typical Physical Properties (measured per ASTM D751)
TEST METHOD
Zytron® 500
Grab Tensile Strength MD*
80 / 359
Grab Tensile Strength CD*
73 / 325
Tear Resistance MD*
27 / 120
Trapezoid Method CD*
15 / 67
Ball Burst
79 / 351
Sources for all test data are independent laboratories. All tests were performed under laboratory conditions and not under actual use conditions.
Agent testing was conducted at Battelle Labs in accordance with MIL-STD-282 and/or NFPA 1994-2001 Edition Standard on Protective Ensembles for Chemical / Biological Terrorism Incidents.